Model
|
Al2O3 |
ZrO2 |
| 99.7% |
96% |
92% |
Al2O3
+ZrO2 |
ZrO2
+Y2O3 |
ZrO2
+MgO |
|
Density (g/cm3)
|
3.93 |
3.72 |
3.65 |
4.00 |
6.01 |
5.60 |
|
Bending Strength (kg/mm2)
|
40 |
35 |
35 |
50 |
90 |
60 |
|
Vickers Hardness(kg/mm2)
|
1,800 |
1,400 |
1,500 |
1,700 |
1,400 |
1,500 |
|
Fracture Toughness(MPam1/2 )
|
3.0 |
2.7 |
2.5 |
4.5 |
7.0 |
8.0 |
|
Thermal Shock Resistance(ΔT)
|
200 |
200 |
200 |
300 |
250 |
400 |
|
Working Temperature(°C)
|
1,500 |
1,500 |
1,400 |
1,500 |
800 |
1,000 |
Corrosion
Resistance |
Acid |
Exce-
llent |
Good |
Good |
Good |
Good |
Good |
| Alkali |
Exce-
llent |
Good |
Good |
Good |
Good |
Good |
|
Merit
|
High Wear Resistance
High Corrosion Resistance
High Temperature Application |
High Wear
Resistance
High Toughness
Insulation of Heat |
|
Model
|
TiC |
Si3N4 |
SiC |
| Al2O3+TiC |
Si3N4 |
SiAlON |
SiC |
|
Density (g/cm3)
|
4.40 |
3.20 |
3.20 |
3.2 |
|
Bending
Strength (kg/mm2)
|
50 |
80 |
80 |
50 |
|
Vickers
Hardness(kg/mm2)
|
1,700 |
1,600 |
1,650 |
2,800 |
|
Fracture
Toughness(MPam1/2 )
|
4.5 |
6.0 |
6.0 |
2.5 |
|
Thermal Shock
Resistance(ΔT)
|
400 |
750 |
750 |
350 |
|
Working
Temperature(°C)
|
1,000 |
1,100 |
1,200 |
1,400 |
Corrosion
Resistance |
Acid |
Good |
Good |
Good |
Excellent |
| Alkali |
Good |
Good |
Good |
Excellent |
|
Merit
|
High Wear
Resistance
High Electrical
Conductivity |
High Thermal Shock
Resistance
High Temp. Strength
High Wear Resistance |
High Wear
Resistance
High Corrosion
Resistance
High Temp,Strength
Excellent Hardness |
|
|
|
|
| |
|
|
|